LFCSP (lead-frame chip-scale package) is a lead-frame-based plastic package whose footprint is close to the size of the die, which is why it is called chip-scale. Figure 1 shows a to-scale cross-section. Internal interconnection is usually implemented with wire bonds. External electrical connection is made by soldering the peripheral pins to the PCB. In addition to the pins, an LFCSP often has a larger exposed thermal pad that can be soldered to the PCB to improve heat dissipation. Reworking these packages requires controlled heating, careful mechanical handling, and attention to moisture and thermal stress. This article explains the rework flow, board preparation, device removal, and profile calibration needed to remove an LFCSP without damaging the package or the PCB.

Figure 1 | Proportional cross-sectional view of LFCSP
Highlights:
- LFCSP removal requires heating the device until the solder under the pins and under the exposed thermal pad (if the pad is soldered) is liquid; mechanical removal should follow complete solder reflow.
- Dry baking the PCB assembly at 125°C for at least 4 hours is strongly recommended before rework to remove residual moisture and prevent popcorn-effect damage, provided the conditions do not exceed the ratings of other devices on the board; otherwise, use the alternative bake conditions in IPC/JEDEC J-STD-033.
- Rework tool settings and temperature profiles must be calibrated for the device, PCB material, thickness, configuration, and thermal mass. Excessive thermal or mechanical stress can cause delamination, package damage, or die tilt, which complicates failure analysis.
LFCSP Device Rework
After an LFCSP has been assembled on a PCB, a defect found during inspection or test should be corrected by rework: the defective device is removed and replaced with a working device. Before removal, the defective device must be heated until the solder under the pins and under the exposed pad (if the pad is soldered) liquefies. This makes it easier to remove the defective device from the circuit board.
The conventional rework flow includes the following steps:
- Prepare the board.
- Remove the device.
- Clean the PCB pads.
- Apply solder paste.
Inspection
Inspection is the seventh step in the rework flow. Removal can generate mechanical stress on both the LFCSP and the PCB. The defective device should be removed carefully not only to avoid damage to the PCB or neighboring devices but also to avoid damage to the defective device itself, especially when failure analysis is planned. Excessive stress on an LFCSP, for example heating the device above its rated peak temperature or exposing it to high temperature for too long, can cause package delamination or external physical damage (Figures 2 to 4). For a device that will be analyzed further, delamination caused by improper removal makes it harder to identify the true failure mechanism. Proper removal of the defective device is therefore necessary for effective failure analysis.
Improper removal can cause delamination at the LFCSP die pad, as observed by scanning acoustic microscopy (Figure 2).

Figure 2 | Delamination of LFCSP die pad caused by improper removal (observed by scanning acoustic microscopy)
Excessive rework settings can produce external damage that appears as bulging molding compound in a low-magnification side view (Figure 3).

Figure 3 | Low-magnification side view of LFCSP showing damage caused by excessive rework setup (mold compound bulging)
Excessive rework settings can also cause internal damage that appears as die tilt in an X-ray image (Figure 4).

Figure 4 | X-ray image of LFCSP showing internal damage caused by excessive rework setup (die tilt)
Board Preparation
Dry baking the PCB assembly before rework begins is strongly recommended to eliminate residual moisture. If residual moisture is not removed, it can damage the device during reflow through the popcorn effect. Bake the PCB assembly at 125°C for at least 4 hours, provided these conditions do not exceed the rated limits of other devices on the PCB. If those conditions exceed the ratings of other devices, use the alternative bake conditions specified in the joint industry standard IPC/JEDEC J-STD-033.
Device Removal
Different tools can be used to remove the device. Removal may involve heating the device until the solder reflows and then removing the device by mechanical means while the solder is still liquid. A programmable hot-air rework system provides controlled temperature and time settings.
Rework should follow the temperature profile used for device assembly. The rework temperature must not exceed the peak temperature specified on the moisture sensitivity level (MSL) label. Heating time can be shortened, for example in the liquefaction zone, as long as complete solder reflow is achieved. The time spent in the solder reflow zone at peak temperature should be less than 60 seconds. The vacuum pressure of the pick-up tool should be less than 0.5 kg/cm2 to prevent the device from being ejected before full reflow and to avoid pad liftoff. Do not reuse a device that has been removed from a PCB.
Control the rework temperature to avoid damaging the LFCSP and the PCB. Covering the area around the device with heat-resistant tape can provide further protection. Heating the underside of the PCB is also recommended to reduce the temperature difference between the top and bottom of the board and to minimize board warpage.
When defining rework tool settings, calibrate the temperature profile. This calibration is especially important when reworking a specific device for the first time. Calibration is also needed for different body sizes, PCB materials, configurations, and thicknesses because these may have different thermal mass. Calibration must include monitoring temperature, time, and other equipment tool settings; Figure 5 outlines a simplified flow chart for device removal evaluation.

Figure 5 | Simplified flowchart for device removal evaluation
Thermocouples can be mounted on different parts of the board assembly, such as the top of the LFCSP and the top of the PCB (Figure 6 shows an example calibration setup). Analyze the temperature-time curve data to obtain effective device removal parameters from the evaluation.

Figure 6 | Example diagram of device removal calibration setup
Related Reading:
Eight Layout Considerations for Differential Filters on PCBs
Improving PCB Immunity to Power Supply Variations in Converter Systems
PCB Layout for Accurate Temperature Measurement: PCB vs Ambient
Best Grounding Practices for Data Converters: Return Paths and Error Voltage
High-Temperature IC Packaging: Die Attach, Wire Bond, Solder and PCB
isoPower Radiated Emissions: Dense PCB Layout Guide
Buck Regulator PCB Layout and Grounding Guide for Low Noise
PCB Thermal Design: Junction Temperature and Power Dissipation
PBGA Rework Procedure: Removal, Pad Cleaning, Paste and Placement